Mina SatoNovember 15, 20265 min read1 views

At a glance

  • Chinese researchers tie efficiency loss in copper-plated HJT metallization to wear of screen mesh knuckles and propose a 4.7% emulsion coverage design.
  • A team in China has identified progressive wear of screen mesh knuckles as the main cause of efficiency loss when printing photoresist for copper-plated silicon heterojunction solar cells, and showed that adding an emulsion buffer layer with 4.7% coverage held minority carrier lifetime degradation to 0.41% after 10,000 printing cycles.
A fine metal printing mesh hovers just above a reflective silicon wafer, with a thin emulsion layer separating the two under cleanroom lighting.

Researchers in China have traced a gradual loss of conversion efficiency in copper-plated silicon heterojunction (HJT) solar cells to wear of the screen mesh used to apply photoresist, and have proposed a modified screen design that limits the damage.

Screen printing is a standard metallization step, but the mechanical pressure and thermal treatment involved can harm the sensitive passivating contact structures of HJT cells, raising recombination losses and cutting conversion efficiency. The issue is especially relevant to copper-plated HJT devices, which are seen as a route to lower metallization cost and reduced reliance on silver.

Why photoresist printing differs from silver paste printing

Corresponding author Lang Zhou told pv magazine that photoresist printing differs fundamentally from conventional silver paste printing. In silver paste printing, screen openings account for only 2–5% of the total area, and an emulsion layer over the remaining surface keeps the mesh from touching the wafer. Full-area photoresist coating, by contrast, typically uses a screen without emulsion coverage so the resist can be deposited uniformly across the whole wafer, meaning the mesh comes into direct and extensive contact with the wafer on every printing cycle.

Measured losses over 15,000 cycles

Earlier work had shown efficiency declining from 26.2% to 25.7% over 15,000 consecutive printing cycles in commercial solar cell production. The losses were attributed mainly to reductions in open-circuit voltage and fill factor, while short-circuit current density and electrical resistance remained largely unchanged. Minority carrier lifetime degradation increased from 0.61% with a new screen to 11.0% after 15,000 cycles.

Using three-dimensional confocal microscopy, the scientists identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles wear down, their contact area with the wafer increases, placing greater mechanical stress on the passivation layers underneath. Scanning electron microscopy revealed no visible surface scratches, but photoluminescence measurements confirmed higher recombination losses, pointing to damage at the amorphous silicon/crystalline silicon interface.

Emulsion buffer with 4.7% coverage

To prevent direct contact, the researchers added an emulsion buffer layer to the screen so the mesh no longer touches the wafer surface. They evaluated six patterns with emulsion coverage ratios ranging from 2.9% to 16.6%.

The results showed a trade-off: higher coverage reduced mechanical damage but impaired photoresist coating uniformity by disrupting ink distribution. A coverage ratio of 4.7% provided the best balance, limiting minority carrier lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good coating uniformity. The team attributed the improvement to the emulsion layer blocking mesh-to-wafer contact and thereby reducing cumulative mechanical damage to the sensitive passivation layers.

Zhou said the findings indicate that a comparatively simple change to screen design can substantially mitigate printing-induced degradation, offering a practical way to improve the manufacturing reliability of copper-plated HJT solar cells.

The work appears in Solar Energy as “Screen-printing photoresist induced efficiency degradation and mitigation in Cu-plated SHJ solar cells.”

Momentum behind copper metallization

The result comes as copper attracts growing interest as an alternative to silver contacts in HJT cells. In April 2026, researchers at China’s Nankai University reported a silver-free HJT cell with 25.2% efficiency, using plasma-induced interface engineering and copper electroplating; the approach addressed adhesion, contact resistance and stability challenges at the ITO interface. Separately, scientists at Germany’s Forschungszentrum Jülich reached 23.08% efficiency in a fully copper-metallized HJT cell — a relatively small penalty compared with its silver-metallized counterpart — while cells combining silver-copper paste on the front side with silver contacts on the rear reached 23.95%. Both results underline copper’s potential to reduce silver consumption, although further improvements in processing and electrical performance remain necessary.

Reported by Mina Sato, Grid Integration, Monitoring and EV Charging Editor.